SmCo Ring Magnet/Permanent Samarium Cobalt Ring Magnets

SmCo Ring Magnet/Permanent Samarium Cobalt Ring Magnets

$0.10 | 1 piece (Min.Order)

Characteristics: 1、The SmCo Magnet has high magnetic performance (high Br, Hcb & (BH) max), reaching the (BH) max of 35MGOe under room temperature, which is only lower than NdFeB magnet, but much higher than other magnets. 2、The working temperature of the SmCo magnet can reach 550℃ that is...
Add To Cart
Chat Now
Description
Technical Parameters

Samarium cobalt ring magnet, also known as SmCo ring magnet, is a commonly used magnetic material, and its chemical composition is SmCo5 or Sm2Co17. SmCo magnets have excellent magnetic properties, high coercive force, oxidation resistance, and corrosion resistance, so they are widely used in electrical, electronic, computer technology, aerospace and other fields.

The manufacturing process of samarium-cobalt ring magnets is relatively complicated, and multiple processes such as pressing and sintering are required during manufacture. Samarium cobalt ring magnets are mainly divided into two types, namely coaxial type and split shaft type. The SmCo Ring Magnet are divided into inner circle, inner circle and outer circle and inner circle, inner circle and outer circle, while split-axis type refers to the combination of two magnets magnetized in different directions.

Samarium cobalt ring magnets are widely used, for example, in motors, generators, computer hard drive read/write heads, antennas, sensors, medical equipment, aerospace and other fields. Samarium-cobalt ring magnets have stable magnetic properties, corrosion resistance, high temperature resistance, and radiation resistance, making them irreplaceable in the design of high-performance electronic devices.

Characteristics

1、The SmCo Ring Magnet has high magnetic performance (high Br, Hcb & (BH) max), reaching the (BH) max of 35MGOe under room temperature, which is only lower than NdFeB magnet, but much higher than other magnets.

2、The working temperature of the SmCo magnet can reach 550℃ that is the highest among all other magnets.

3、The SmCo Ring Magnet has strong corrosion resistance and anti-oxidation, which can be used for a durable time.

4、The SmCo Ring Magnet has an extremely low temperature coefficient, generally -0.030%/K.




Hot Tags: smco ring magnet, China smco ring magnet suppliers, manufacturers, Flexible NdFeB Magnet, Magnetic Filter, Ferrite Magnet Pot, Tailing Recovery PM Separator, Rubber Magnet Block, NdFeB Magnet Holder

Typical Magnetic Performance for SmCo magnet

Material

Grade

Remanence

Coercive Force

Intrinsic Coercive

Max Energy

Working Temp

Br

Hcb

Hcj

(BH)max

T

KGs

KA/m

KOe

KA/m

KOe

KJ/m³

MGOe

SmCo5

XG18

0.85-0.90

8.5-9.0

650-700

8.3-8.8

1194-1830

15-23

127-143

16-18

≤250

SmCo5

XG20

0.90-0.94

9.0-9.4

666-725

8.5-9.1

1194-1830

15-23

143-159

18-20

≤250

SmCo5

XG22

0.94-0.97

9.4-9.7

700-748

8.9-9.4

1194-1830

15-23

159-175

20-22

≤250

SmCo5

XG24

0.97-1.02

9.7-10.2

720-780

9.2-9.7

1194-1830

15-23

175-195

22-24

≤250

SmCo5

XG18H

0.85-0.90

8.5-9.0

650-700

8.3-8.8

≥1830

≥23

127-143

16-18

≤250

SmCo5

XG20H

0.90-0.94

9.0-9.4

666-725

8.5-9.1

≥1830

≥23

143-159

18-20

≤250

SmCo5

XG22H

0.94-0.97

9.4-9.7

710-748

8.9-9.4

≥1830

≥23

159-175

20-22

≤250

SmCo5

XG24H

0.97-1.02

9.7-10.2

730-780

9.2-9.8

≥1830

≥23

175-195

22-24

≤250

Sm2Co17

XGS20L

0.90-0.94

9.0-9.4

533-732

6.7-9.2

636-955

8-12

143-159

18-20

≤250

Sm2Co17

XGS22L

0.94-0.97

9.4-9.7

533-740

6.7-9.3

636-955

8-12

159-175

20-22

≤250

Sm2Co17

XGS24L

0.97-1.02

9.7-10.2

541-756

6.8-9.5

636-955

8-12

175-191

22-24

≤250

Sm2Co17

XGS26L

1.02-1.05

10.2-10.5

541-764

6.8-9.6

636-955

8-12

191-207

24-26

≤250

Sm2Co17

XGS28L

1.05-1.08

10.5-10.8

541-780

6.8-9.8

636-955

8-12

207-223

26-28

≤250

Sm2Co17

XGS30L

1.08-1.11

10.8-11.1

541-796

6.8-10.0

636-955

8-12

223-239

28-30

≤250

Sm2Co17

XGS32L-A

1.11-1.13

11.1-11.3

549-804

6.9-10.1

636-955

8-12

239-255

30-31

≤250

Sm2Co17

XGS32L-B

1.13-1.145

11.3-11.45

550-805

6.9-10.1

636-955

8-12

246-262

31-32

≤250

Sm2Co17

XGS20M

0.90-0.94

9.0-9.4

637-732

8.0-9.2

955-1433

12-18

143-159

18-20

≤300

Sm2Co17

XGS22M

0.94-0.97

9.4-9.7

645-740

8.1-9.3

955-1433

12-18

159-175

20-22

≤300

Sm2Co17

XGS24M

0.97-1.02

9.7-10.2

661-764

8.3-9.6

955-1433

12-18

175-191

22-24

≤300

Sm2Co17

XGS26M

1.02-1.05

10.2-10.5

685-788

8.6-9.9

955-1433

12-18

191-207

24-26

≤300

Sm2Co17

XGS28M

1.05-1.08

10.5-10.8

693-812

8.7-10.2

955-1433

12-18

207-223

26-28

≤300

Sm2Co17

XGS30M

1.08-1.11

10.8-11.1

700-828

8.8-10.4

955-1433

12-18

223-239

28-30

≤300

Sm2Co17

XGS32L-A

1.11-1.13

11.1-11.3

812-860

10.2-10.8

≥1433

≥18

239-255

30-31

≤300

Sm2Co17

XGS32L-B

1.13-1.145

11.3-11.45

820-870

10.3-10.9

≥1433

≥18

239-255

31-32

≤300

Sm2Co17

XGS20

0.90-0.94

9.0-9.4

653-732

8.2-9.2

≥1433

≥18

143-159

18-20

≤300

Sm2Co17

XGS22

0.94-0.97

9.4-9.7

677-740

8.5-9.3

≥1433

≥18

159-175

20-22

≤300

Sm2Co17

XGS24

0.97-1.02

9.7-10.2

693-772

8.7-9.7

≥1433

≥18

175-191

22-24

≤300

Sm2Co17

XGS26

1.02-1.05

10.2-10.5

748-796

9.4-10.0

≥1433

≥18

191-207

24-26

≤300

Sm2Co17

XGS28

1.05-1.08

10.5-10.8

756-820

9.5-10.3

≥1433

≥18

207-223

26-28

≤300

Sm2Co17

XGS30

1.08-1.11

10.8-11.1

788-836

9.9-10.5

≥1433

≥18

223-239

28-30

≤300

Sm2Co17

XGS32-A

1.11-1.13

11.1-11.3

812-860

10.2-10.8

≥1433

≥18

239-255

30-31

≤300

Sm2Co17

XGS32-B

1.13-1.145

11.3-11.45

820-870

10.3-10.9

≥1433

≥18

239-255

31-32

≤300

Sm2Co17

XGS20H

0.90-0.94

9.0-9.4

661-732

8.3-9.2

≥1990

≥25

143-159

18-20

≤350

Sm2Co17

XGS22H

0.94-0.97

9.4-9.7

685-740

8.6-9.3

≥1990

≥25

159-175

20-22

≤350

Sm2Co17

XGS24H

0.97-1.02

9.7-10.2

700-772

8.8-9.7

≥1990

≥25

175-191

22-24

≤350

Sm2Co17

XGS26H

1.02-1.05

10.2-10.5

756-796

9.5-10.0

≥1990

≥25

191-207

24-26

≤350

Sm2Co17

XGS28H

1.05-1.08

10.5-10.8

765-820

9.6-10.3

≥1990

≥25

207-223

26-28

≤350

Sm2Co17

XGS30H

1.08-1.11

10.8-11.1

796-836

10.0-10.5

≥1990

≥25

223-239

28-30

≤350

Sm2Co17

XGS32-A

1.11-1.13

11.1-11.3

820-860

10.3-10.8

≥1990

≥25

239-255

30-31

≤350

Sm2Co17

XGS32-B

1.13-1.15

11.3-11.5

830-880

10.4-11.0

≥1990

≥25

246-262

31-32

≤350

Sm2Co17

XGS16LT

0.81-0.85

8.1-8.5

605-669

7.6-8.4

≥1592

≥20

111-127

14-16

≤300

Sm2Co17

XGS18LT

0.85-0.90

8.5-9.0

629-708

7.9-8.9

≥1592

≥20

127-143

16-18

≤300

Sm2Co17

XGS20LT

0.90-0.94

9.0-9.4

661-732

8.3-9.2

≥1592

≥20

143-159

18-20

≤300

Sm2Co17

XGS22LT

0.94-0.97

9.4-9.7

685-740

8.6-9.3

≥1592

≥20

159-175

20-22

≤300


Physical properties of SmCo magnet

Material

Modulus of

elasticity

Ultimate

tensile

strength

Density

Electrical Resistivity

Curie

temperature

Recoil

permeability

Temp. Coeff. of Br

SmCo5

23 x 106 psi

6 x 103 psi

8.2 g/cm3

5 µ-ohm-cm/cm2

700-750

1.00-1.05

-0.045% /

Sm2Co17

17 x 106 psi

5 x 103 psi

8.4 g/cm3

86 µ-ohm-cm/cm2

800-850

1.00-1.10

-0.03 % /